Is it the same pads consistently pulling off and are the pads connected to
traces?
Toby
On Mar 27, 2012 2:19 PM, "Leland Woodall" <[log in to unmask]> wrote:
> Folks,
>
> We've ran across a strange incident and I'd like a little advice from the
> group.
>
> We recently underwent a component vendor change, and part of the first
> group of boards were misbuilt due to incorrect polarity (the part marking
> was misinterpreted by the vision operator).
>
> Anyway, an attempt to remove the part by our Repair group resulted in
> lifted pads on 10 of the first 12 boards. We've analyzed the lead material
> beneath the SEM and it returns 98% tin and 2% silicone. The old style
> component comes off quite easily (within 3 seconds), and an analysis of its
> leads shows to be 100% tin. It's a 6 pin diode with very little mass.
>
> What's going on here? Does a 2% silicone mix raise the melting point of
> solder by 200 degrees C?
>
> Please help me understand.
>
> Thanks,
>
> Leland
>
> ________________________________
>
> “Confidentiality Notice:
> This transmission (including any attachments) may contain confidential
> information belonging to the sender and is intended only for the use of the
> party or entity to which it is addressed. If you are not the intended
> recipient, you are hereby notified that any disclosure, copying,
> distribution, retention or the taking of action in reliance on the contents
> of this transmission is strictly prohibited. If you have received this
> transmission in error, please immediately notify the sender and erase all
> information and attachments.”
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|