TECHNET Archives

March 2012

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Leland Woodall <[log in to unmask]>, TechNet E-Mail Forum <[log in to unmask]>
Date:
Tue, 27 Mar 2012 17:42:15 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Toby Carrier <[log in to unmask]>
Message-ID:
Subject:
From:
Toby Carrier <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="windows-1252"
MIME-Version:
1.0
Parts/Attachments:
text/plain (53 lines)
Is it the same pads consistently pulling off and are the pads connected to
traces?

Toby
On Mar 27, 2012 2:19 PM, "Leland Woodall" <[log in to unmask]> wrote:

> Folks,
>
> We've ran across a strange incident and I'd like a little advice from the
> group.
>
> We recently underwent a component vendor change, and part of the first
> group of boards were misbuilt due to incorrect polarity (the part marking
> was misinterpreted by the vision operator).
>
> Anyway, an attempt to remove the part by our Repair group resulted in
> lifted pads on 10 of the first 12 boards.  We've analyzed the lead material
> beneath the SEM and it returns 98% tin and 2% silicone.  The old style
> component comes off quite easily (within 3 seconds), and an analysis of its
> leads shows to be 100% tin.  It's a 6 pin diode with very little mass.
>
> What's going on here?  Does a 2% silicone mix raise the melting point of
> solder by 200 degrees C?
>
> Please help me understand.
>
> Thanks,
>
> Leland
>
> ________________________________
>
> “Confidentiality Notice:
> This transmission (including any attachments) may contain confidential
> information belonging to the sender and is intended only for the use of the
> party or entity to which it is addressed. If you are not the intended
> recipient, you are hereby notified that any disclosure, copying,
> distribution, retention or the taking of action in reliance on the contents
> of this transmission is strictly prohibited. If you have received this
> transmission in error, please immediately notify the sender and erase all
> information and attachments.”
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2