TECHNET Archives

October 2012

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Glidden, Kevin" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Glidden, Kevin
Date:
Wed, 17 Oct 2012 18:19:05 +0000
Content-Type:
text/plain
Parts/Attachments:
text/plain (29 lines)
 Never heard of such a thing....but what about a dip in ESD floor paint?


-----Original Message-----
From: Douglas Pauls [mailto:[log in to unmask]] 
Sent: Wednesday, October 17, 2012 2:09 PM
To: [log in to unmask]
Subject: [TN] ESD Heat Shrink Sleeving

Good afternoon all,

I wonder if any of you know of  a heat shrinkable sleeving that would be in the static dissipative range for volume resistivity?  This would be between 1E6 and 1E9 ohm-cm.  Most of the ones that I am aware of are 1E11 ohm-cm or higher.

I don't know of any, so I thought I would turn to my favorite forum. 

The application is paint brush handles.  Since most brushes are painted wood, they can generate static.  We thought having a shrinkable ESD cover, vs. some of the liquid coatings, would be a possible solution.

Doug Pauls


______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] ______________________________________________________________________

______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

ATOM RSS1 RSS2