Good afternoon all,
I wonder if any of you know of a heat shrinkable sleeving that would be
in the static dissipative range for volume resistivity? This would be
between 1E6 and 1E9 ohm-cm. Most of the ones that I am aware of are 1E11
ohm-cm or higher.
I don't know of any, so I thought I would turn to my favorite forum.
The application is paint brush handles. Since most brushes are painted
wood, they can generate static. We thought having a shrinkable ESD cover,
vs. some of the liquid coatings, would be a possible solution.