We have made a composition analysis of our solder wave solder pot and
discovered a deviation of the SnPB content. The Sn percentage had gone up to
65.45% and the Pb content down to 34.54%. I suppose there will be a (small)
change in the constitutional behaviour of the alloy - some bigger range of
the liquid-to-solid stage. Except this, what should we be aware of in
practice in regards to solder joint quality and reliability? We continue to
maintain the pot temperature at 250 deg C (482 deg F).

Any inputs will be appreciated!

Best regards,
Yordan Venev

********************************************************
CENTILLION LTD.
7-th km Tzarigradsko shosse Blvd.
ATM Center
1784 Sofia, BULGARIA
Tel. :(+359 2) 974 47 51, 965 84 95, 965 58 85
Fax :(+359 2) 974 47 52
mail to: [log in to unmask]
www.centillion-bg.com



---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2