This must be a problem season :
after flakes, cabbages and roses , I have this copper "boulders" alloy
problem :
On our routine microsectioning of (4umNi + 0.3umAu; 63/37) joints we
discovered we have rather interesting phenomenon :
After the obvious dissolution of gold ; there are sitting on top of Nickel
(admittedly bit thin ; still , continuous) microcracked boulders (about same
dia as the Ni layer) .
when we zoomed scan on them ; we found they're CuSn alloy ! Looks like a
smallpoxed nickel face .
Now our regular profiling 's telling us we're nowhere near this alloying
scenarios ;
and we ponder about the cracking propagations ; the Q is :
Where are this aliens coming from ?
Contaminants of tubs from some previous process ?
Smudged sample polish ?
Appears only on one specific fab supply .
Paul Klasek
http://www,resmed,com
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################
|
|
|