TECHNET Archives

February 2001

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Robert Lazzara <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Mon, 12 Feb 2001 10:42:48 EST
Content-Type:
text/plain
Parts/Attachments:
text/plain (33 lines)
In a message dated 2/12/01 10:07:41 AM, [log in to unmask] writes:

<< What about any traces or ground planes which are not covered with

solder mask?  These locations would not get solder coated, therefore would

remain IWT.  Wouldn't there be a concern of tin whisker growth over time in

the field? >>

James, wait: Your application is going beyond the intent of the material. IWT
is not applied to the PWB as a post assembly finish. IWT, like your other
interest OSP, are designed to preserve a solderable pre-assembly finish,
nothing more. Tin whiskering becomes moot as there would be worse things
waiting for immersion and organic coatings after assembly.

The idea of using immersion coatings or OSP as a post assembly finish is, in
my opinion, a bad idea. This will be argued by people who have had OSP coated
groundplanes on backpanels in the tropics since 1975, but I won't put my
warranty on it.

Robert Lazzara

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2