TECHNET Archives

October 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Phil Hinton <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Mon, 4 Oct 2004 12:35:26 EDT
Content-Type:
text/plain
Parts/Attachments:
text/plain (29 lines)
The banding probably does not come from the pulse plating, banding is often
seen in nickel plating without pulse plating and was quire common in the days
of pyrophoshate copper plating also without pulse plating . Overdosing of some
additive/leveler.brighteners will cause banding even in acid copper plate  The
banding due to bath chemistry is seen most often as 6 to 15 bands in about
1.5 mils. of plating.  It is most prevalent at the corners of the holes and
these corners often crack when subjected solder float testing.  The cause of the
banding is the reneucleation of the plating several times during the plating
process, eah reneucleation cause a new band .  It most often occurs with
overdosing brighteners or by running the bath too long with out treatment or cleanup.


Banding due to pulse plating is often not detectable as it would happen at
about 100-300
bands in the the 1.5 mils of plating.      .

Phil Hinton
Hinton PWB Engineering

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2