Bread tins will work and the fan to enhance cooling is also good. The suggestion of peanut oil may work, but remember it will smoke, so be sure to watch the smoke alarms and sprinklers.
If you have a fire ext near by be sure it is "dry power" not CO2 or water.
Randy
----- Original Message -----
From: Steve Gregory
To: [log in to unmask]
Sent: Friday, August 23, 2002 11:00 AM
Subject: Re: [TN] Emptying wave solder pot
Hi Bev!
No I'm not pulling your leg. This was when I was out in California working for Comptronix (they got bought by Sanmina).
I remember that I was sceptical too, molten solder in a cardboard container, but it worked. The containers scorched a bit, but they held the solder. Of course they didn't fill them very full, less than half-way up of a 1-gallon container.
I've got almost 1500-lbs. I've got to empty from the pot, and I'm just trying to think of something that will make things go a little quicker. I plan to reuse most of the solder in our new machine that we're getting, along with some virgin bars. Our new wave has a 1800-lb. pot!
-Steve Gregory-
Steve,
Are you pulling our collective leg?! Molten solder at 235C is darn close to good ole Fahrenheit 451 (good book). Yeah, yeah, I know it is cooling and is closer to 190 C, but... Or is this "can" treated with non-flammable fillers and maybe a inner metal coating? Why not just use new paint cans?
Bev
-----Original Message-----
From: Steve Gregory [mailto:[log in to unmask]]
Sent: August 23, 2002 8:46 AM
To: [log in to unmask]
Subject: [TN] Emptying wave solder pot
Hi All!
In a couple of weeks, I'm going to have to empty the wave solder pot on our Treiber.
In the past, I remember round cardboard containers being used to put the solder in after ladling it from the pot. Does anybody know where I can get those?
Thanks!
-Steve Gregory-
--------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|