I'm looking for information on intermetallic growth, for a good solder
joint, what is acceptable and what is unacceptable as being too low or too
high.
As far as I know, it depends on the elements and thermal cycles.
Assume: Cu-Sn63Pb37 and NiAu-Sn63Pb37,
90 seconds in liquidus, 2 thermal cycles.
How does the intermetallic thickness change if I had to change the paste
from eutectic to Ag2-Sn-Pb? (not even to mention lead-free paste)
Is there any formula that can help in undestanding what would be the
intermetallic thickness if I had to undergo another thermal cycle, or if I
had to change the liquidus time on my oven profile?
Any information will be very welcome.
Thanks,
Ivanoe
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|