TECHNET Archives

May 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Thu, 23 May 2002 13:01:13 -0400
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Torres, Roberto" <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="iso-8859-1"
From:
"Torres, Roberto" <[log in to unmask]>
Parts/Attachments:
text/plain (90 lines)
Ryan;

Thanks for the information, as this is not my are of expertise, I
was concerned about the several thousand hours. Is there some documentation
that has information on how different material hold up under extended
periods
of time under these conditions?

Again thanks for you help.

Regards
Bob Torres

-----Original Message-----
From: rgrant [mailto:[log in to unmask]]
Sent: Thursday, May 23, 2002 9:38 AM
To: 'TechNet E-Mail Forum.'; 'Torres, Roberto'
Subject: RE: [TN] PCB materials


Bob,  What you are asking for is not exotic.  Board fab processes, and PCB
assembly processes will have a bigger impact under those conditions than the
raw materials in the PCB.  Standard FR-4 and your favorite finish (including
OSP covered copper) will work just fine.

Regards,
Ryan Grant

-----Original Message-----
From: Torres, Roberto [mailto:[log in to unmask]]
Sent: Wednesday, May 22, 2002 12:53 PM
To: [log in to unmask]
Subject: [TN] PCB materials


All;

I am looking for some help in selecting material for a PCB we are
designing to go into 85/85 (85°C / 85% humidity), aging (85°C dry bake), and
temp cycle (-40°C to 85°C) ovens. I know that there are dozens of options
out there for fabricating boards that will survive this, but I'm sure that
some of them are considered standard processes that can be obtained
inexpensively, and some of them more exotic. Could any of you offer some
guidance?  One of my biggest concerns is the metallization in the
high-humidity environment.  I think that copper could cause some serious
problems here... but under a mask and with SnPb on all the exposed areas,
maybe I'm wrong. Each of the boards must last a minimum of 1000 hours at
these conditions, although several thousands of hours is obviously
preferable, so that they can be reused.  

Any help provided would be greatly appreciated.

Regards
Bob Torres

Roberto Torres
CENiX Inc.
5141 California Ave, Suite 150
Irvine, CA 92612
Email: [log in to unmask]
Tel:     949-428-2672 
Fax:    949-428-2671 

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET
Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------