Subject: | |
From: | |
Reply To: | TechNet E-Mail Forum. |
Date: | Thu, 29 Aug 2002 10:12:11 +0200 |
Content-Type: | multipart/alternative |
Parts/Attachments: |
|
|
I don't see how the manufacturer could win. The part with missing bonds doesn't show that there were bonds before in the location with missing bonds, and the gap in the broken bonds is too large to be induced by the assembly or ICT process. I suppose that the x-ray was taken before decapsulation.
The only thing they could say is about the cracks- which can be seen only after decapsulation, and may be induced during this process. But I am sure that your failure analysis lab people are fair enough to have told you that if it happened.
Gaby
----- Original Message -----
From: Steve Gregory
To: [log in to unmask]
Sent: Thursday, August 29, 2002 5:20 AM
Subject: Re: [TN] MUX Failures...an update to the last update
So Earl,
We all see that, how do you address this problem with the OEM? I ask that question subjectively...
You have to know that we've already done that, and we're being blamed for handling....hehehe.
This is the "Kobiashu Maru" scenario that I spoke of earlier. This is a no-win scenario. On Semiconductor will have all their legal staff (which is more substantial than most of us ever have) to support their position that their parts are okay...so we have to deal with it. We'll eat all the costs that we will incur from their sub-standard processes and won't be able to do anything about it...
As a note, comparible Fairchild MUX's work GREAT!!!
(that's been backed-up by test data...)
-Steve Gregory-
In a message dated 8/28/2002 7:56:33 PM Central Daylight Time, [log in to unmask] writes:
again, possible wire bond crash and burn. something's amiss in the process.
MoonMan
--------------------------------------------------------------------------------- Technet Mail List provided as a free service by IPC using LISTSERV 1.8e To unsubscribe, send a message to [log in to unmask] with following text in the BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest Search the archives of previous posts at: http://listserv.ipc.org/archives Please visit IPC web site http://www.ipc.org/html/forum.htm for additional information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315 ---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|