Greg,
I've seen this type of thing happen, where a silver filled die
attach adhesive (probably through silver migration) shorted to
traces below the die. We mostly make ceramic hybrids, so our
solution was to use a couple of layers of glass encapsulant
(designed for encapsulating fired resistors, and not containing any
pin holes) as a die pad. The glass encapsulant does have to be
fired at a high temperature (800 C or so), so it is only a solution for
ceramic substrates.
Brett Goldstein
EVI, Inc.
> Hi Designers,
>
> I'm in need of help! I have completed a design with some L157
> IC's
> on the Board. And Manufacturing came back to me after I finished the
> design and was about to ship it and said that they use a conductive epoxy
> to adhere the die to the Board and they're worried that if the Solder
> Resist has pin holes in it that it could leak a signal into the runners
> below those Die. They said they could use Pre-Forms but that would kill
> their yeild so they want me to reroute the traces below those die.
> Unfortuatley that would be a nightmare and add at least a week to my time.
> So can anyone tell me where I can get info to help prove that this won't
> be a problem or are they right and there's a good possiblitiy that this
> could happen.
>
> Thank you,
>
> Greg Bodi
>
> [log in to unmask]
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|