Linda: Do not know if this will work, as it MIGHT not make lines fine enough. We use this pen when we want to make PERMANENT markings on glassware in the lab, and if it is fine enough, it should work very well.
The name is the "Speedry" metal marking pen, made by Ideal.
Similar pen is called MARK-IT marker, by Southern Marking Systems, out of Greenville SC. 864-233-3961 Colors available are white, black, orange, red, yellow.
CHECK to see if any contain Lead!
Rudy Sedlak
RD Chemical Company
--- On Fri, 7/2/10, Linda Langley <[log in to unmask]> wrote:
From: Linda Langley <[log in to unmask]>
Subject: [TN] Silk Screen Ink Pen
To: [log in to unmask]
Date: Friday, July 2, 2010, 9:13 AM
Is there such thing as an ink pen that could be used to touch up flaws
on silk screen letters and numbers? Any idea where I could find
information?
Linda Langley CIT
Training Specialist
Jabil Circuit
248-292-6176
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|