TECHNET Archives

July 2010

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Date:
Mon, 19 Jul 2010 14:52:46 -0700
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, R Sedlak <[log in to unmask]>
Subject:
From:
R Sedlak <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset="utf-8"
MIME-Version:
1.0
Parts/Attachments:
text/plain (62 lines)
So, using the obvious, going to Google, typing in Iodine Gold Etch...
One of the entries was the following:

Gold and iodine form gold iodide via 2 Au + I2 􏰀 2 AuI. 
The solubility of AuI is improved by adding KI to the solution. Iodine/iodide can be substituted by other halogenides excepting fluorine which does not form soluble gold compounds.
In a mixing ratio of   KI:I2 :H2O=4g:1g:40ml, 
[To clarify that is  4 grams KI, 1 gram Iodine, 40 mls water]
a room temperature etch rate of approx. 1 μm/min gold is attained. Copper reveals a comparable etch rate, while nickel is only etched in case of current linkage to gold.
[Note about this last line:  EN is MUCH more corrosion resistant than pure Nickel]

Good luck
Rudy Sedlak

--- On Mon, 7/19/10, Bev Christian <[log in to unmask]> wrote:

From: Bev Christian <[log in to unmask]>
Subject: [TN] Removing gold and leaving nickel unaffected
To: [log in to unmask]
Date: Monday, July 19, 2010, 11:38 AM

TechNetters,
is there a way of chemically removing an ENIG gold layer and not attacking the underlying nickel without using cyanide?
Bev
RIM

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------



      

______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask] 
______________________________________________________________________

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2