TECHNET Archives

June 2001

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Mon, 4 Jun 2001 15:38:53 EDT
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="US-ASCII"
From:
"<Rudy Sedlak>" <[log in to unmask]>
Parts/Attachments:
text/plain (26 lines)
I don't know how much money this will save you...however, for what it is
worth......

Go to a flex PCB manufacturer, have him get some copper foil...no laminate.
(flex guys are set up to handle floppy material like foil)
Put photoresist on one side...plate 0.005 tin lead on the other.
Strip photoresist.
FUSE Tin/Lead, otherwise you have only discrete chrystals of Tin/Lead, not
true alloy.
Etch Copper away....

Hope this helps.

Rudy Sedlak
RD Chemical Company

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2