You might try Alpha Metals at alphametals.com. They're the main solder
suppliers that I know of, but they may not do foils.
Pete Duncan
"Marsico, James"
<James.Marsico@D To: [log in to unmask]
P.AIL.COM> cc: (bcc: DUNCAN Peter/Asst Prin Engr/ST Aero/ST Group)
Sent by: TechNet Subject: [TN] SOLDER FOIL
<[log in to unmask]
>
06/05/01 03:05
AM
Please respond
to "TechNet
E-Mail Forum.";
Please respond
to "Marsico,
James"
I'm looking for a source for foil Sn63 solder, .005" thick, anywhere from 4
to 10 inches wide. I probably need 25 ft, but one of the major solder
suppliers wants a lot charge of $3,000 which will yield around 1400 ft.
Any
suggestions?
Jim Marsico
Senior Engineer
Production Engineering
EDO Electronics Systems Group
[log in to unmask] <mailto:[log in to unmask]>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
---------------------------------------------------------------------------------
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|