Rich,
I haven't seen that specific data. Most Sn-Pb alloy researchers don't worry
about tensile strength so much because other considerations are usually more
important such as creep, creep fatigue, and thermal fatigue. Here are a
couple of references that may help point you to data.
[1] Solder Mechanics - A State of the Art Assessment, D.R. Frear, W.B.
Jones, and K.R. Kinsman, TMS 1991, ISBN0-87339-166-7.
[2] Solder Joint Reliability - Theory and Applications, edited by John
H. Lau, Van Nostrand Reinhold, 1991, ISBN 0-442-00260-2.
You might contact Kester, Alpha Metals and/or Indium Corporation and ask
them for this data.
Best Regards,
Ed Hare, PhD
http://www.semlab.com
-------------------------------------------------------------
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Richard Kraszewski
Sent: Wednesday, October 27, 2004 3:48 PM
To: [log in to unmask]
Subject: [TN] Solder Strength over temperature
I'm looking for information pertaining to the tensile strengths of 63/37,
90/10 and 95/5 solder alloys over temperature. Preferably for ~-20C to 125C.
Any information where I could find this would be greatly appreciated.
Rich K / KEDS
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e To
unsubscribe, send a message to [log in to unmask] with following text in the
BODY (NOT the subject field): SIGNOFF Technet To temporarily halt or
(re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet
NOMAIL or (MAIL) To receive ONE mailing per day of all the posts: send
e-mail to [log in to unmask]: SET Technet Digest Search the archives of
previous posts at: http://listserv.ipc.org/archives Please visit IPC web
site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|