TECHNET Archives

October 2004

TechNet@IPC.ORG

Options: Use Proportional Font
Show HTML Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Scott B. Westheimer" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Scott B. Westheimer
Date:
Sat, 16 Oct 2004 20:19:53 -0400
Content-Type:
text/plain
Parts/Attachments:
text/plain (50 lines)
Unetched copper bridging between two features. This should be caught if you
are using AOI Gerber compare.


Scott B. Westheimer
----- Original Message -----
From: "Bhaskar.C.S" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Saturday, October 16, 2004 5:25 AM
Subject: [TN] internal shorts in MLB'S


What are the various reasons for getting internal shorts in Multilayer
Pcb's?


REGARDS

D.VENKATESWARLU

--
This message has been scanned for viruses and
dangerous content by OpenProtect(http://www.openprotect.com), and is
believed to be clean.


---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2