Sorry Bev, I am guilty of using terminology that is specific to my end of
the industry. Hot air leveling (HAL) leaded, means that the surface finish
is tin lead , I defined it as leaded because there is a leaded as well as
non-leaded surface finish out there now. This is a military account so we
cannot use no-lead. I did leave out the materials used typically it has been
FR4, 130 as well as 170.
Sorry.
Bill
----- Original Message -----
From: "Bev Christian" <[log in to unmask]>
To: <[log in to unmask]>; <[log in to unmask]>
Sent: Monday, June 15, 2009 10:53 AM
Subject: Re: [TN] HAL-Leaded assembly
Bill,
Not enough info!
What surface finish?
What board type?
What environment boards stored in?
How long between manufacture of boards and use?
Bev
RIM
----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Mon Jun 15 13:47:51 2009
Subject: [TN] HAL-Leaded assembly
Hello everybody, I am looking for some knowledge on what I see is a basic
type problem that is driving me crazy. I am a sales guy who covers a sizable
territory and in that territory for a PCB manufacturer (yes one of those) I
have one account that I have been working with for about 4 years now that
continuously has issues assembling both hand assembly as well as pick &
place.
The surface finish is HAL (leaded) this is a military account that is pretty
well structured in their processes. What I get told is that there seems like
a contamination is on the surface when they scrub the surface it makes it
better but not 100% better.They have sent back samples for us to look at ,
we saw nothing on the surface no contamination nothing wrong at all.
If this was one of a few that has the same or similar issues it would make
some sense and I could go to the people I work with asking them to look into
this issue. But it is the only company that has this issue.
Has anybody seen a similar type of a situation before? Understood that you
cannot fix this but would appreciate advise as to where to look so hopefully
this can be solved.
Thank you.
Bill Dworak
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential
information, privileged material (including material protected by the
solicitor-client or other applicable privileges), or constitute non-public
information. Any use of this information by anyone other than the intended
recipient is prohibited. If you have received this transmission in error,
please immediately reply to the sender and delete this information from your
system. Use, dissemination, distribution, or reproduction of this
transmission by unintended recipients is not authorized and may be unlawful.
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|