TECHNET Archives

June 2009

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, Bill Dworak <[log in to unmask]>
Date:
Mon, 15 Jun 2009 14:27:39 -0400
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Bev Christian <[log in to unmask]>
Subject:
From:
Bev Christian <[log in to unmask]>
content-transfer-encoding:
quoted-printable
In-Reply-To:
A<A93CE567CAFB4AFAAC023264BBFC67CA@dell>
Content-Type:
text/plain; charset="us-ascii"
MIME-Version:
1.0
Parts/Attachments:
text/plain (145 lines)
Bill,
No prob. I should have been able to figure that out. I'm just used to
seeing HASL.
Bev

-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Bill Dworak
Sent: Monday, June 15, 2009 2:16 PM
To: [log in to unmask]
Subject: [TN] Fw: [TN] HAL-Leaded assembly

Sorry Bev, I am guilty of using terminology that is specific to my end
of 
the industry. Hot air leveling (HAL) leaded, means that the surface
finish 
is tin lead , I defined it as leaded because there is a leaded as well
as 
non-leaded surface finish out there now. This is a military account so
we 
cannot use no-lead. I did leave out the materials used typically it has
been 
FR4, 130 as well as 170.
 Sorry.

 Bill


----- Original Message ----- 
From: "Bev Christian" <[log in to unmask]>
To: <[log in to unmask]>; <[log in to unmask]>
Sent: Monday, June 15, 2009 10:53 AM
Subject: Re: [TN] HAL-Leaded assembly


Bill,
Not enough info!
What surface finish?
What board type?
What environment boards stored in?
How long between manufacture of boards and use?
Bev
RIM

----- Original Message -----
From: TechNet <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Sent: Mon Jun 15 13:47:51 2009
Subject: [TN] HAL-Leaded assembly

Hello everybody, I am looking for some knowledge on what I see is a
basic 
type problem that is driving me crazy. I am a sales guy who covers a
sizable 
territory and in that territory for a PCB manufacturer (yes one of
those) I 
have one account that I have been working with for about 4 years now
that 
continuously has issues assembling both hand assembly as well as pick & 
place.
The surface finish is HAL (leaded) this is a military account that is
pretty 
well structured in their processes. What I get told is that there seems
like 
a contamination is on the surface when they scrub the surface it makes
it 
better but not 100% better.They have sent back samples for us to look at
, 
we saw nothing on the surface no contamination nothing wrong at all.
If this was one of a few that has the same or similar issues it would
make 
some sense and I could go to the people I work with asking them to look
into 
this issue. But it is the only company that has this issue.
 Has anybody seen a similar type of a situation before? Understood that
you 
cannot fix this but would appreciate advise as to where to look so
hopefully 
this can be solved.
Thank you.

 Bill Dworak

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to 
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to 
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 
for additional information, or contact Keach Sasamori at [log in to unmask]
or 
847-615-7100 ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential 
information, privileged material (including material protected by the 
solicitor-client or other applicable privileges), or constitute
non-public 
information. Any use of this information by anyone other than the
intended 
recipient is prohibited. If you have received this transmission in
error, 
please immediately reply to the sender and delete this information from
your 
system. Use, dissemination, distribution, or reproduction of this 
transmission by unintended recipients is not authorized and may be
unlawful. 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------

---------------------------------------------------------------------
This transmission (including any attachments) may contain confidential information, privileged material (including material protected by the solicitor-client or other applicable privileges), or constitute non-public information. Any use of this information by anyone other than the intended recipient is prohibited. If you have received this transmission in error, please immediately reply to the sender and delete this information from your system. Use, dissemination, distribution, or reproduction of this transmission by unintended recipients is not authorized and may be unlawful.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2