TECHNET Archives

August 1999

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Sender:
Subject:
From:
Joe Aronson <[log in to unmask]>
Date:
Tue, 17 Aug 1999 16:29:51 +0100
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset=US-ASCII
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Joe Aronson <[log in to unmask]>
Parts/Attachments:
text/plain (63 lines)
Rudy,

Thanks for the reply.  I have seen this application in a horizontal spray etching chamber and it seemed to provide enough of a break in the solution bridge tro minimize the effect.  Is this your experience also?

Joe


>>> Rudy Sedlak <[log in to unmask]> 08/17/99 10:15AM >>>
Joe:

Deepest sympathy.  You are fighting a no-win battle.  There really is no
known answer.  As long as electrons can travel from a more active Copper
site, to a less active Gold site, and both touch the same etch solution,
you've got a terribly lopsided etch.

The reason, is that the reaction of the oxidizer, be it Peroxide, or
Persulfate, or Cupric, or???, tends to interfere with, and thus slow down the
metal dissolution.  When you have a gold pad electrically connected to a
Copper surface, the Peroxide/Persulfate reaction occurs all on the Gold pad,
and the Copper surface is free to dissolve unimpeded, and it does!

One wild, and weird way that one customer resolved this issue was to get rid
of microetching.  That involved some serious re-engineering, but it can be
done.

Save eliminating microetch, the only way to resolve this is to cover the Gold
with something non-conductive.  (This sounds expensive)

If you want to discuss, call me, or mail me at work.

Rudy Sedlak
RD Chemical Company
650-962-8004
[log in to unmask] 

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Gayatri Sardeshpande at [log in to unmask] or
847-509-9700 ext.5365
##############################################################

ATOM RSS1 RSS2