TECHNET Archives

January 2003

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
"Furrow, Robert Gordon (Bob)" <[log in to unmask]>
Reply To:
TechNet E-Mail Forum.
Date:
Fri, 10 Jan 2003 15:26:38 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (67 lines)
Carrie,

It has been our experience that with Via in Pad product this high a solder
pot temperature can create fractures of the solder joint of surface mount
components on the topside. I believe IBM put out a paper describing this
phenomena and called the failure "double reflow". We found BGAs also
susceptible to this if the traces to the vias on the outer rows were too
short. I would recommend keeping the pot temperature as low as good process
results allow.

Thanks,
Robert Furrow
Printed Wiring Board Engineer
Supply Chain Networks
Lucent Technologies
978-960-3224    [log in to unmask]


-----Original Message-----
From: Morse, Carrie [mailto:[log in to unmask]]
Sent: Friday, January 10, 2003 3:15 PM
To: [log in to unmask]
Subject: [TN] Wave Temperature


As I sit here on a Friday afternoon with little time to start thinking about
questions that would be great for a "PCB Assembly Trivial Pursuit" game, I
thought of something.

At what temperature does everyone run their Sn63Pb37 wave machine....and
Why?

We run ours at 260C, but, don't know why.  We started to get into the
discussion as to why, and, some of the reasons were: 1) That's what was
recommended, 2)It's hot enough to burn off the flux, 3)It reduces surface
tension.

Can someone enlighten us?

Thanks,
Carrie

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
-----------------------------------------------------

---------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
-----------------------------------------------------

ATOM RSS1 RSS2