TECHNET Archives

September 1998

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Content-Type:
text/plain
Sender:
Subject:
From:
"Crepeau, Phil" <[log in to unmask]>
Date:
Thu, 10 Sep 1998 07:43:10 -0700
MIME-Version:
1.0
X-To:
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, "Crepeau, Phil" <[log in to unmask]>
Parts/Attachments:
text/plain (79 lines)
hi,

as you are probably aware, the curing agent has a very large effect on
the properties of the cured system.  if you haven't had luck with a
manufacturer of molding compounds for these components, you should try
the shell chemical web site at:

http://www.shellchemical.com/

go to their products section and look for epon resins.  there are also
email addresses and telephone nos. for you to use.  they should be of
help.

phil crepeau

-----Original Message-----
From: Clive Ffitch [mailto:[log in to unmask]]
Sent: Wednesday, September 09, 1998 4:45 PM
To: [log in to unmask]
Subject: [TN] Biphenol Resins


     All,

     Can anyone supply typical values for the following thermal
properties
     of Biphenol Resins, as used for PED/PEM (particularly surface mount
     package) moulding compounds?

     I've searched all my usual sources, but only have figures for the
     (more common?) Epoxy Cresol Novalac Resins:

     Moulding Compound:         TCE:          Therm.Cond:        Tg:
                         (ppm x 10^6/degC)     (W/mdegC)       (degC)

----------------------------------------------------------------------
     Epoxy Cresol                16               0.67          155
       Novalac Resin      (some up to 20)                 (some up to
200)


     Biphenol Resin              ?                 ?             ?


     Thanks for any figures/information,

     Regards all,

     Clive ffitch
     Matra BAe Dynamics (UK)
     Stevenage, England

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
################################################################

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2