Anne,
I couldn't find any definitions for CTI, but I did find some people who were
spec'ing it for different materials used in electronics/electrical usage.
The CTI was specified in Volts, and the people who specified it said it was
tested using the following standards:
UL746
DIN 53480
IEC 60664-1
IEC 60664-3
I didn't have much luck finding these standards, but maybe that will help
you in your search.
Thomas DeSmit
EDA Librarian/Sr. Engineering Tech.
IFR Americas, INC.
The opinions expressed are my own, and do not necessarily reflect those of
my employer.
> -----Original Message-----
> From: TechNet E-Mail Forum. Anne Ledger <[log in to unmask]>
> [mailto:[log in to unmask]]
> Sent: Thursday, March 18, 1999 10:21 AM
> To: [log in to unmask]
> Subject: [TN] Comparative Tracking Index?
>
>
> Good Morning TechNet,
>
> I have a fabrication drawing with a note with the following note.
>
> Material: .062 laminated glass (woven fabric) base, epoxy resin, Flame
> retardent, FR4.
> copper clad 2 oz./sq ft. Laminate must be certified to
> have a minimum comparative
> tracking index of 175. Microsection demonstrating
> compliance with copper weight,
> dielectric spacing, line width and use of CTI 175 or
> better material shall be shipped
> with each lot.
>
> I am at a loss on the CTI 175 stuff. I have reviewed IPC 4101 and don't
> find a reference. I have
> placed a call to our material supplier but no response yet. The TechNet
> seems much faster.
> Can anyone provide me with a clue? Thanks in advance for the help.
>
> Anne Ledger
> EMDS, Inc.
> [log in to unmask]
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC's web site (http://www.ipc.org) "On-Line
> Services" section for additional information.
> For technical support contact Hugo Scaramuzza at [log in to unmask]
> or 847-509-9700 ext.312
> ################################################################
>
>
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################
|
|
|