IPC-A-610 4.2.4.2 Hardware Mounting - Hole Obstruction of Solder Fill.
Process Indicator Class 2
Defect Class 3
Parts and components prevent fill of plated-through holes that are required
to be soldered.

 Guy Ramsey
American Competitiveness Institute
Senior Lab Technician / Instructor
610 362-1200 ext 107


-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Edward Brunker
Sent: Wednesday, October 04, 2000 8:10 AM
To: [log in to unmask]
Subject: [TN] Pin in Hole


If a connector body is pushed flush to the PCB, does this present any
difficulties for pin in hole?
Regards
Edward Brunker
Principal Process Engineer

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2