Subject: | |
From: | |
Reply To: | TechNet E-Mail Forum. |
Date: | Tue, 24 Oct 2000 07:58:26 -0400 |
Content-Type: | text/plain |
Parts/Attachments: |
|
|
Do you clean after each solder cycle or only after the wave solder cycle?
Guy Ramsey
American Competitiveness Institute
Senior Lab Technician / Instructor
610 362-1200 ext 107
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Pelchat, Janice
Sent: Friday, October 20, 2000 1:04 PM
To: [log in to unmask]
Subject: [TN] OSP boards and White residue
I read through some archives on OSP boards but didn't find as much as I
think I may need.
We have OSP boards that are run through topside reflow, bottomside reflow,
wave solder processes. These processes use water based pastes/fluxes.
(Which I gather may be the cause of the residue?)
The residue we see is not very prominent - seems to "outline" or shadow the
circuitry if you will.
What are other experiences with OSP finishes and white residues? Do you
let go as is? The residue is permanent and does not come off with Proclean
or aqueous wash.
Jan Pelchat
----------------------------------------------------------------------------
-----
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF TECHNET
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF TECHNET
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|