Hi Steve,
According to my copy of MIL-P-13949H there is no "E" special consideration
1.2.1.1.1.3:
N P K L M G T J
Unless they changed something in an amendment.
Hans
~~~~~~~~~~~~~~~~~~~
Hans M. Hinners
Materials Engineer (Process & Manufacturing)
Warner Robins Air Logistics Center
Avionics Production Division
Precision Attack/ Radar/Manufacturing Branch
Engineering Section
380 Second Street, Suite 104
Building: 640, Mail Stop: LYPME
Robins AFB, GA 31098-1638
Voice: (478) 926 - 1970 Fax: (478) 926 - 7164
mailto:[log in to unmask]
http://www.robins.af.mil
-----Original Message-----
From: Stephen R. Gregory [mailto:[log in to unmask]]
Sent: Wednesday, September 20, 2000 1:01 PM
To: [log in to unmask]
Subject: [TN] Mil laminate designations...
Hi all!!
What does the last "E" in the Mil designation type "GEE" laminate stand for?
I though it was the color...for instance "GEN" would be a G-10 natural
color,
right?
Also, is there any real difference in "GE" vs. "GF" laminate material?
Thanks!
-Steve Gregory-
##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8d
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe: SUBSCRIBE TECHNET <your full name>
To unsubscribe: SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################
|
|
|