Eric,
I am still hunting for good net sites for your first request.

With regards to the latter:
No, bismuth is not more toxic.  Bismuth oxychloride is used in the cosmetics
industry and other bismuth salts (I forget which one(s)) are used in
PeptoBismol® (Did I spell that right?)  No bismuth compounds are listed in
the 1990 "NIOSH Pocket Guide to Chemical Hazards" I have and only bismuth
telluride is listed in the ACGIH TLV Booklet - because of the tellurium.
Toxicity does come into play in its mining, though, as 10 to 40% (depends on
who you talk to and/or whether you are talking world-wide or country
specific) comes as a by-product of lead mining.

regards,
Bev Christian
Research in Motion

-----Original Message-----
From: Eric Christison [mailto:[log in to unmask]]
Sent: December 7, 2001 11:36 AM
To: [log in to unmask]
Subject: [TN] Info on lead free reflow profiles sought


After half an hour's fruitless searching of the net I thought of Technet.

Can anyone out there point me at a web page or email me a reflow profile for
one of the higher
melting point lead free solders. I'm trying to produce a test spec to
determine whether some
temperature sensitive components would survive a 'worst case' reflow cycle.

By the way. I note that many of the lead free alloys contain Bismuth. Isn't
this more toxic
than lead? Am I being naive in my surprise that one toxic chemical is being
replaced with
something equally bad?

Regards,

----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2