After half an hour's fruitless searching of the net I thought of Technet.
Can anyone out there point me at a web page or email me a reflow profile for one of the higher
melting point lead free solders. I'm trying to produce a test spec to determine whether some
temperature sensitive components would survive a 'worst case' reflow cycle.
By the way. I note that many of the lead free alloys contain Bismuth. Isn't this more toxic
than lead? Am I being naive in my surprise that one toxic chemical is being replaced with
something equally bad?
Regards,
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------