Hi Russ,
I used to run about 1.3-1.5N and about 165g/l Cu with an ORP of 550-580 or
so. It would seem to me that the parameters you listed would lead to a
very fast but somewhat less precise etchant. You may experience undercut
and/or poor conductor edge quality. And you're right about potential
equipment problems, particularly titanium shafts, nuts, bolts, etc. But it
would be fast......... If you're working with 1/4 ounce copper you may want
to stand back a few feet to catch the layers as they fly off.....
Check with Mr. Sedlak..... he is The Man for cupric questions.
Mark
At 10:14 AM 11/28/01 -0800, you wrote:
>----Thanks to everyone for the info , I was a weak on Cupric, (I spent
>my life using mostly Ammonium and Ferric, amongst other more exotic
>etches)
>
>Any way one more simple or not so simple question :
>
> Would you run a Cupric etcher @ 140g/l Cu and 5N HCl .?
>
> Is It a correct assumption that somewhat lower N, and higher
>copper would , provide faster etch rate. It just seems to me that
>operating at an extreme N will basically just cost money in the form of
>excess HCL usage , not to mention the wear and tear on the equipment,
>and operators.,
>
>
>Again thanks for the information!
>
>Russell Smith
>
>
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|