Hi Steve,
Thanks for the prompt response.
What kind of solder thieves should I put in, say a SOIC08? Do I need to put in
leading pads and leading pads? Is there any standard published that I can find
or buy regarding wave soldering issues?
Thanks for the support.
Patrick
Steve Owen <[log in to unmask]> on 10/23/2001 09:03:04 AM
Please respond to "TechNet E-Mail Forum." <[log in to unmask]>
To: [log in to unmask]
cc: (bcc: Patrick Lam/SEL)
Subject: Re: [TN] Land pattern for wave soldering
Hi Patrick,
If you look at say a side one footprint(reflow)for quad flat pack as opposed
to a side two (wavesolder)side. On side two you will ideally need to present
the component @ 45 deg to the wave and have solder thieves in each of the
four corners to eliminate solder bridges.
just an example.
hope its of some use.
-----Original Message-----
From: Patrick Lam [mailto:[log in to unmask]]
Sent: 23 October 2001 16:26
To: [log in to unmask]
Subject: [TN] Land pattern for wave soldering
Hi Technetters,
Is there a need to have different SMD land size/ pattern for wave soldering?
Any
suggestion is appreciated.
Thanks,
Patrick
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|