Henry,
Have you tried using frame racks. Custom racks that clamp a layer
on all 4 sides. I've done work plating .005" core for burried and blind
vias
using these it worked well.
John Haman Jr.
----------
> From: Henry Coulter <[log in to unmask]>
> To: [log in to unmask]
> Subject: [TN] Plating thin, less than .005", via layers
> Date: Wednesday, March 25, 1998 12:21 PM
>
> I regularly need to clamp via layers (PWB's) to unclad fiberboard frames
> before pattern plating. We currenty use platers' tape to attach the via
> to the frame, it works well but it's too time consuming. Does anyone
> have a better way to do this? Is there a clamping device out there?
> Will appreciate any sugestions.
> Henry Coulter
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional
information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
847-509-9700 ext.311
> ################################################################
>
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|