Steve, Ed
I have also participated in mass addition of wires to fix design issues,
without impact to reliability. But the two cents I want to add is that
it's OK to do a jumper as a repair for a damaged trace IF you know why
the trace is damaged (e.g.. physical damage). If you blindly add
jumpers to fix mystery opens in a board then you may be sending walking
wounded out to the field to die later.
As always: opinions are my own, mileage may vary; contents are hot, not
suitable for small children...
regards,
Graham Collins
Process Engineer
Litton Systems Canada
(902) 873-2000 extension 215
> -----Original Message-----
> From: SteveZeva [SMTP:[log in to unmask]]
> Sent: Wednesday, March 25, 1998 5:03 PM
> To: [log in to unmask]
> Subject: Re: [TN] circuit board trace repair
>
> Ed,
>
> At a past employer, we built boards for a pretty large networking
> company
> that went into one of their servers. Because of mistake in one of the
> Gerber
> files for a assembly, we had to do a trace cut and install a jumper
> wire as
> part of the normal production process, which to me, would be the same
> as a
> trace repair.
>
> From what I know, everything was fine with the boards...they ran
> just
> like they were supposed to and never had any problems. I know this is
> not
> scientific data, but just something that may show that if the repair
> is done
> correctly there shouldn't be a problem whatsoever...
>
> -Steve
> Gregory-
>
> ################################################################
> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
> 1.8c
> ################################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
> following text in the body:
> To subscribe: SUBSCRIBE TechNet <your full name>
> To unsubscribe: SIGNOFF TechNet
> ################################################################
> Please visit IPC web site (http://jefry.ipc.org/forum.htm) for
> additional information.
> For the technical support contact Dmitriy Sklyar at [log in to unmask] or
> 847-509-9700 ext.311
> ################################################################
################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe: SUBSCRIBE TechNet <your full name>
To unsubscribe: SIGNOFF TechNet
################################################################
Please visit IPC web site (http://jefry.ipc.org/forum.htm) for additional information.
For the technical support contact Dmitriy Sklyar at [log in to unmask] or 847-509-9700 ext.311
################################################################
|
|
|