TECHNET Archives

March 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Mime-Version:
1.0
Content-Type:
text/plain; charset=us-ascii
References:
Date:
Tue, 25 Mar 1997 08:56:15 -0500
Precedence:
list
Resent-From:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
reply-to:
X-Mailing-List:
<[log in to unmask]> archive/latest/11439
From [log in to unmask] Tue Mar 25 11:
37:21 1997
TO:
Return-Path:
<TechNet-request>
Status:
O
X-Loop:
Received:
by ipc.org (Smail3.1.28.1 #2) id m0w9WRO-000BikC; Tue, 25 Mar 97 07:39 CST
Resent-Message-ID:
<"qBZYt2.0.ZjB.vLzDp"@ipc>
Subject:
From:
"George Franck" <george@[11.1.1.33]>
Old-Return-Path:
In-Reply-To:
[log in to unmask] (Timothy Gaylor) "Microsectioning" (Mar 24, 7:40pm)
X-Mailer:
Z-Mail for Macintosh (3.2.2 19Jun95)
Message-Id:
Parts/Attachments:
text/plain (28 lines)
I have always prefered the NH3 H2O2 etch.  But as you found out,
it has a limited shelf life.  Because of this, (in a past life)
we would mix up a few drops at a time in a watch glass as needed,
and dip the sections in the watch glass.  In these volumes,
evaporation tended to keep the solution fresh.  And  when it all
evaporated, well, make up another 10 drop batch.  So we had a
small bottle of NH3 and one of H2O2 at the grinding table, with a
watch glass and paper towels.  One used q-tips, the others just
dipped in the watch glass.  

-- 
George Franck
Principal Product Engineer
Raytheon E-Systems
Falls Church Va

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2