I would say you are running a big risk. Why? Imagine your cleaning
process is good and gives, say, 0.5 µg/cm² eq. NaCl, which you deem by
qualification to be very good. You then make a few hand solder joints,
with the flux spread over, say, 1 cm², out of a total of 250 cm² for the
whole board. Your ionics now read 0.55 µg/cm² eq. NaCl and you say,
"Whacko! Jolly Good! Eveything in the garden is lovely!" But is it? That
rise of 0.05 µg/cm² relates to only 1 cm² but is divided by 250 cm², so
the real contamination level where your hand soldered joints are will be
12.5 µg/cm² eq. NaCl. Are you going to sleep so peacefully knowing
this? I wouldn't! :-(
Brian
Joel Alexander wrote:
> We are processing some assemblies with water soluble flux that requires
> washing. We then wash the assemblies as required by C-22. The next step
> we add a some hand soldered parts with no clean VOC flux but do not clean
> the assembly. We sample test the boards for ionic contamination and they
> pass.
>
> Should these be considered compliant since they pass or would the no-clean
> solder have to also be washed of.
>
> FYI this is for some military work.
>
> Any help would be appreciated
>
> Joel Alexander
>
> APSCO Quality Assurance Manager
>
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
>
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|