TECHNET Archives

December 2006

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Date:
Fri, 1 Dec 2006 16:02:19 +0200
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, Brian Ellis <[log in to unmask]>
Subject:
From:
Brian Ellis <[log in to unmask]>
Content-Transfer-Encoding:
quoted-printable
In-Reply-To:
Content-Type:
text/plain; charset=ISO-8859-1; format=flowed
MIME-Version:
1.0
Parts/Attachments:
text/plain (52 lines)
I would say you are running a big risk. Why? Imagine your cleaning 
process is good and gives, say, 0.5 µg/cm² eq. NaCl, which you deem by 
qualification to be very good. You then make a few hand solder joints, 
with the flux spread over, say, 1 cm², out of a total of 250 cm² for the 
whole board. Your ionics now read 0.55 µg/cm² eq. NaCl and you say, 
"Whacko! Jolly Good! Eveything in the garden is lovely!" But is it? That 
rise of 0.05 µg/cm² relates to only 1 cm² but is divided by 250 cm², so 
the real contamination level where your hand soldered joints are will be 
  12.5 µg/cm² eq. NaCl. Are you going to sleep so peacefully knowing 
this? I wouldn't! :-(

Brian

Joel Alexander wrote:
> We are processing some assemblies with water soluble flux that requires
> washing.   We then wash the assemblies as required by C-22.  The next step
> we add a some hand soldered parts with no clean VOC flux but do not clean
> the assembly. We sample test the boards for ionic contamination and they
> pass.
> 
> Should these be considered compliant since they pass or would the no-clean
> solder have to also be washed of.
> 
> FYI this is for some military work.
> 
> Any help would be appreciated
> 
> Joel Alexander
> 
> APSCO Quality Assurance Manager
> 
> ---------------------------------------------------
> Technet Mail List provided as a service by IPC using LISTSERV 1.8e
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
> -----------------------------------------------------
> 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2