In the past, I have sent back old solder paste to our bar solder supplier with
our dross.  I got rid of old paste, didn't have to worry about scrapping
hazardous materials and they paid us for the "scrap" metal.
Just a thought.

K McCoy - 
Rockwell Automation/Allen-Bradley

_______________________________________________________________________________
From: ddhillma on Thu, Dec 12, 1996 8:00 PM
Subject: Re: Assy: Solder Paste in Wave Solder Pots...
To: [log in to unmask]
Cc: [log in to unmask]

     Hi Steve -
     
     Well, your wave solder pot will get pretty messy, definitely smell 
     bad/different for a period of time and you will generate quite a bit 
     of excess dross but I believe that as long as the solder alloy 
     originally met the ANSIJ-STD-006 specification requirements you won't 
     introduce any metallic type contamination that would cause you solder 
     joint reliability concerns. Have fun(??), wear a mask, and let us know 
     what happens.
     
     
     Dave Hillman
     Rockwell Collins
     [log in to unmask]


______________________________ Reply Separator
_________________________________
Subject: Assy: Solder Paste in Wave Solder Pots...
Author:  [log in to unmask] at ccmgw1
Date:    12/12/96 3:42 PM


     
Good day all!
     
    This might seem like a pretty dumb question, but I was wondering if
there's 
anything wrong with putting old solder paste in yer' wave solder pot? I was 
feeling bored the other day, so I cleaned out our solder paste 'fridge, and
I've
got some jars of a bunch of different samples of no-cleans and water solubles 
that were played around with in the past, and I just want to get rid of them 
before an operator grabs one and uses it. They're all the same alloy (63/37)
but
there are different flux types. We're in a water soluble process now, and we 
don't build missile guidance systems, just class-II stuff.
     
    I wouldn't think it would hurt anything, but I don't wanna' do it if
there's
something I'm not thinking about and I wind-up contaminating the pot
somehow... 
(BOY, the operations boss would have my "keester"!!!) 
     
    Any problems with doing that? I mean with adding old paste to the solder 
pot? NOT with kicking my keester if I contaminated the solder pot...heck, I 
would kick my OWN keester if I did that...heh,heh...
     
     
     
                                          __\/__
                                      .  / ^  _ \  .
                                      |\| (o)(o) |/|
                            #------.OOOo----oo----oOOO.-----#
                            #        Steve Gregory          #
                            #  [log in to unmask]    #
                            #                               #
                            #________________Oooo.__________#
                                      .oooO  (   )
                                      (   )   ) /
                                       \ (   (_/
                                        \_)
     
*************************************************************************** 
* TechNet mail list is provided as a service by IPC using SmartList v3.05 * 
*************************************************************************** 
* To unsubscribe from this list at any time, send a message to:           * 
* [log in to unmask] with <subject: unsubscribe> and no text.        * 
*************************************************************************** 
* If you are having a problem with the IPC TechNet forum please contact   * 
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      * 
***************************************************************************
     

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************


------------------ RFC822 Header Follows ------------------
Received: by mke9.ra.rockwell.com with ADMIN;12 Dec 1996 19:59:58 -0600
Received: by moat.ra.rockwell.com; id TAA28256; Thu, 12 Dec 1996 19:59:57
-0600
Received: from ipc.org(168.113.24.64) by moat.ra.rockwell.com via smap (3.2)
	id xma028226; Thu, 12 Dec 96 19:59:30 -0600
Received: from ipc.org by simon.ipc.org via SMTP (940816.SGI.8.6.9/940406.SGI)
	 id TAA21553; Thu, 12 Dec 1996 19:46:29 -0800
Resent-Date: Thu, 12 Dec 1996 19:46:29 -0800
Received: by ipc.org (Smail3.1.28.1 #2)
	id m0vYL3J-0000b4C; Thu, 12 Dec 96 18:00 CST
Resent-Sender: [log in to unmask]
Old-Return-Path: <[log in to unmask]>
Date: Thu, 12 Dec 96 17:00:19 cst
From: "ddhillma" <[log in to unmask]>
Encoding: 67 Text
Message-Id: <[log in to unmask]>
To: [log in to unmask]
Cc: [log in to unmask]
Subject: Re: Assy: Solder Paste in Wave Solder Pots...
Resent-Message-ID: <"z4zxj1.0.6mB.fn9io"@ipc>
Resent-From: [log in to unmask]
X-Mailing-List: <[log in to unmask]> archive/latest/8521
X-Loop: [log in to unmask]
Precedence: list
Resent-Sender: [log in to unmask]

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To unsubscribe from this list at any time, send a message to:           *
* [log in to unmask] with <subject: unsubscribe> and no text.        *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2