We are using white tin "Omikron", have been for a few years.
Benefits: Flat surface, Less shorts, fewer problems screen printer and P&P
equipment in finding
Fiducials. I recommend you try it.
Chris
-----Original Message-----
From: richard wiltron [SMTP:[log in to unmask]]
Sent: Monday, August 20, 2001 2:03 PM
To: [log in to unmask]
Subject: [TN] White Tin
Dear Net member,
Ever heard of white tin finish used in place of HASL?
I heard it's pretty good and there's no lead.
Opinions? Wanna test it?
Your help in this matter is greatly appreciated!!!
Thanks,
Richard
__________________________________________________
Do You Yahoo!?
Make international calls for as low as $.04/minute with Yahoo!
Messenger
http://phonecard.yahoo.com/
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV
1.8d
To unsubscribe, send a message to [log in to unmask] with following
text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message:
SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources &
Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
information, or contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|
|
|