Hi Craig,
so how long is a piece of string?
As a generalisation, non-ionic surfactants used are;
nonyl phenyl alkoxylates
polyprop/polyeth ABA co-polymers
alkylenic ethoxylates
fluorinated esters
The latter two are commonly used.
If you want to give me more info I can perhaps help you more specifically.
Take this offline if you want.
Best regards,
Andrew Hoggan
BBA Associates Ltd
www.bba-associates.ltd
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Craig Hillman
Sent: 16 August 2001 16:59
To: [log in to unmask]
Subject: [TN] Wetting Agents
Hello Technetter,
Quick question: What are some of the common chemicals used as wetting
agents/surfactants in fluxes?
Thanks for your help,
Craig
-----Original Message-----
From: TechNet [mailto:[log in to unmask]]On Behalf Of Furrow, Robert Gordon
(Bob)
Sent: Wednesday, August 15, 2001 2:31 PM
To: [log in to unmask]
Subject: [TN] FMA Labs in Northeast US
Hi All,
With the drastic reduction occurring here at Lucent, I am going to be
without the services of our Evaluation / FMA Lab in Princeton for (at the
very least) the period it takes to relocate it. At the worst, it could be
shut down altogether. I am looking for another source to do the testing of
PWB's and Backplanes for conformance to our specifications and reliability
needs. This testing includes cross-sectioning with analysis, XRF, thermal
shock, pull tests, solderability evaluation, SIR/EM, SEM/EDX, and also FMA
of assembled boards. Ideally, I am looking for someone within driving
distance so that I can easily foster the relationship. However, I am open to
any viable suggestions. If this is a testimonial from users please respond
via the TechNet. If this is a lab promoting its capabilities, please contact
me directly at [log in to unmask] Thanks in advance for everyone's input.
P.S. I am also looking for a lab to provide me the direction, insight,
foresight, enthusiasm, and overall experience that George Wenger at our
Princeton Lab has provided me.
Thanks,
Robert Furrow
Printed Wiring Board Engineer
Strategic Supply Global Account Manager
Supply Chain Networks
Lucent Technologies
978-960-3224 [log in to unmask]
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
----------------------------------------------------------------------------
-----
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET
Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases >
E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700
ext.5315
----------------------------------------------------------------------------
-----
---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send the following message: SET Technet NOMAIL
Search previous postings at: www.ipc.org > On-Line Resources & Databases > E-mail Archives
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------
|