Looks like the glass encapsulation does not extend over the end of the
package.
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of stephengregory5849
Sent: Tuesday, February 09, 2010 12:08 AM
To: [log in to unmask]
Subject: Re: [TN] Rough surface of glass diode (Fairchild 1N4148)
Hi David,
Just finished wave soldering a bunch of boards tonight, and got a chance to
post your pictures. They are here:
http://stevezeva.homestead.com/files/Fairchild_1N4148.jpg
http://stevezeva.homestead.com/files/Shiny_surface.jpg
http://stevezeva.homestead.com/files/Rough_surface.jpg
Looks like solder to me. Have you taken a solder iron to it and see if it
liquifies? Don't know how that would happen, and really don't know if that
is going to be a problem with the lead to glass seal. Doesn't look right to
me...
Steve
----- Original Message -----
From: Dave He
To: 'stephengregory5849' ; 'TechNet E-Mail Forum'
Sent: Monday, February 08, 2010 6:06 PM
Subject: FW: Rough surface of glass diode (Fairchild 1N4148)
Hi Steve,
Could you post the pictures when you get a chance? Thanks.
All,
Two different surfaces were found on Fairchild glass diode (1N4148), one
end is the regular shiny surface while the other end is a flat, rough
surface. Later please see pictures for details.
What is the rough surface? How is it formed? Does it functionally affect
the performance and reliability?
I guess it's formed during molding, but not sure. I send the pictures to
Fairchild but they want some parts back to analyze before tell what it is.
Anyone saw this before? Thanks.
Regards,
Dave He
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------
______________________________________________________________________
This email has been scanned by the MessageLabs Email Security System.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|