I am not an expert in this area but there might be an acceptable work round
if you have trouble sourcing suitable material

1) ensure the mesh  (of conveyor) or inside of machine is earthed/grounded 
2)Blow with an ioniser [at the end of the tunnel] or introduce ioniser into
air path.

I am surprised to hear there is a charge. Work I did with an EFD supplier
some years ago showed that there wouldn't be as the turbulence from the
drying fans generated enough ions not just to carry charge to the work but
also gave a path for dissipation from it. Maybe fan designs have changed or
something.  We also found that there most certainly couldn't be any residual
charge by doing the above (even with artificially charged samples).

A thought anyway for comment if nothing else.


Regards 

Mike Fenner 
Indium Corporation 

T: + 44 1908 580 400
M: + 44 7810 526 317 
F: + 44 1908 580 411 
E: [log in to unmask] 
W: www.indium.com 
Pb-free: www.Pb-Free.com 
-----
SMART 6th European Conference, Brighton 16-18 November 2004
www.smartgroup.org/con2004/conference2004.pdf




-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Rick Thompson
Sent: Tuesday, November 02, 2004 1:26 AM
To: [log in to unmask]
Subject: [TN] Aqueous cleaner mats??


We have traditionally used mesh mats in our aqueous cleaner baskets for
protection of small boards. These mats were made out of polypropylene (sp?)
but recently a customer requested that we remove them for ESD concerns
because a charge can be measured on them when exiting the cleaners after
hot-air drying. The only ESD matting we've been able to locate is somewhat
absorbent and tends to become saturated with contaminants over time.  Does
anyone know of any matting that is ESD safe but not absorbent?  I believe
the mats we originally used are fairly common in use; is there documented
evidence that the charge that registers on them is not sufficient to cause
any damage?
 
Thanks in advance for any insights.
 
 
Rick Thompson
Sr. SMT Process Engineer
SMTEK International
 
+1 (805) 532-2800   x-193
[log in to unmask]
 
 
_ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _ _

This e-mail and any files transmitted with it are confidential and
intended solely for the use of the individual or entity to whom
they are addressed.
If you have received this e-mail in error please notify the
originator of the message. This footer also confirms that this
e-mail message has been scanned for the presence of computer viruses.

Any views expressed in this message are those of the individual
sender, except where the sender specifies and with authority,
states them to be the views of SMTEK International Inc.

Scanning of this message and addition of this footer is performed
by SurfControl E-mail Filter software in conjunction with 
CA e-trust anti-virus detection software.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16
for additional information, or contact Keach Sasamori at [log in to unmask] or
847-615-7100 ext.2815
-----------------------------------------------------


:::::::::::::::::::::::::::

This email, its content and any files transmitted with it are intended solely for the addressee(s) and may be legally privileged and/or confidential. If you are not the intended recipient please delete and contact the sender by return and delete the material from any computer. Any review, retransmission, dissemination or other use of, or taking of any action in reliance upon, this information by persons or entities other than the intended recipient is prohibited.

Messages sent via this medium may be subject to delays, non-delivery and unauthorized alteration. This email has been prepared using information believed by the author to be reliable and accurate, but Indium Corporation makes no warranty as to accuracy or completeness. In particular, Indium Corporation does not accept responsibility for changes made to this email after it was sent. Any opinions or recommendations expressed herein are solely those of the author. They may be subject to change without notice.

:::::::::::::::::::::::::::

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2