TECHNET Archives

April 1997

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Received:
by ipc.org (Smail3.1.28.1 #2) id m0wHJK1-000BisC; Tue, 15 Apr 97 20:15 CDT
From [log in to unmask] Wed Apr 16 10:
15:12 1997
Old-Return-Path:
Date:
Tue, 15 Apr 97 20:27 EST
Precedence:
list
X-Loop:
Resent-Sender:
TechNet-request [log in to unmask]
X-Status:
Status:
O
X-Mailing-List:
<[log in to unmask]> archive/latest/12005
TO:
ipctech email <[log in to unmask]>
Return-Path:
<TechNet-request>
Resent-Message-ID:
<"XslFQ1.0.haJ.yW2Lp"@ipc>
Subject:
From:
Bernard Kessler & Associates LTD <[log in to unmask]>
Resent-From:
Message-Id:
Parts/Attachments:
text/plain (38 lines)
Hi----- from Jurassica----

An over-simplified response to ------ G10 / FR4 (the Flame Retardant G-10) (old
NEMA designations ----- equivelant to the original Mil Spec designations of 
GE and GF respectively ----

Considering G10 as the basic epoxy glass laminate, the FR4 was considered the
G10 with Flame Retardant characteristics.   The Mil spec permitted certification
of the higher level in a hierarchy of products to pertain to the products on the
lower levels and did permit certification of the GF to pertain to GE callouts on
contract drawings.

The differences in performance or processing was invariably a function of how
the laminator achieved the flame-retardant properties ---- what modifications
were made to the epoxy resin formula.  Essentially, however, the properties for
which one selected epoxy glass laminates---- certain mechanicals and moisture
resistance amongst others ----  were not compromised by the flame-retardant
characteristic.

This is a broad stroke reply ----- the supplier in the case noted was correct in
what he did.

Best to all---

Bernie Kessler

***************************************************************************
* TechNet mail list is provided as a service by IPC using SmartList v3.05 *
***************************************************************************
* To subscribe/unsubscribe send a message <to: [log in to unmask]>   *
* with <subject: subscribe/unsubscribe> and no text in the body.          *
***************************************************************************
* If you are having a problem with the IPC TechNet forum please contact   *
* Dmitriy Sklyar at 847-509-9700 ext. 311 or email at [log in to unmask]      *
***************************************************************************



ATOM RSS1 RSS2