TECHNET Archives

March 1999

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Paul Klasek <[log in to unmask]>
Date:
Tue, 16 Mar 1999 16:43:16 +1300
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, Justin Braime <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="iso-8859-1"
From:
Justin Braime <[log in to unmask]>
Parts/Attachments:
text/plain (272 lines)
As far as I'm aware we're allowed to just pump our fumes straight out, here
in 'clean, green' New Zealand. Mind you, the NZ goverment banned all leaded
fuel here a couple of years back, so I guess it's only a matter of time
before Australian enviromental laws spill over here. I think we'll be
looking at filtration for our exhaust stacks real soon...

Justin Braime
Process Engineer - Compuspec Industries

-----Original Message-----
From: Paul Klasek <[log in to unmask]>
To: [log in to unmask] <[log in to unmask]>
Date: Tuesday, March 16, 1999 3:35 PM
Subject: Re: [TN] Solder Fumes


>100 Ton's per year !?! ; far out ; looks like IBM itself is exempt !
>"Small guys" processing less than 100 000 kg's (are we on metric tone ? ;
>close anyhow ?) of solder per year !
>Well , have to admit, I don't fit to jap cars (height 'm talkin bout here,
>ok ?) ;
>so I'm really trying to comprehend the scope of your "exhaustive" answer ,
>if yo' know what I mean .
>Somehow my flabbergastation is gettin' worst still !
>
>See you                paul
>
>PS
>Nothing taken literally buddy ; going to hit the beach at sunset ; to
ponder
>over life in LA .
>Being on top of food chain accumulations 's got lesser risks here by the
>feel of it ;
>apart from steroids from beef and antibiotics disfunctions from poultry .
>But : as Patrick said ; fallin' accidentally the Empire Building, passin'
>each window :
>"So far so good"
>
>> ----------
>> From:         Stephen R. Gregory[SMTP:[log in to unmask]]
>> Sent:         Tuesday, 16 March 1999 5:16
>> To:   [log in to unmask]
>> Subject:      Re: [TN] Solder Fumes
>>
>> In a message dated 3/15/99 8:37:29 AM Pacific Standard Time,
>> [log in to unmask] writes:
>>
>> << Hi Todd&Russ&Steve&Bev
>>
>> Just a point when you've raised the 6 month screening (quite right) : Few
>> HR
>> dept.s have the foresight of screening NEWCOMERS ; and occasionally get
>> company into serious poo when a fellow tramping for decades over silicon
>> valley with all of the chimneys for pigeon eradicating programs ; (I
don't
>> believe my eyes here as I read all of this ;you guys have it way too easy
>> over
>> there ; we have to have by law [not every buddy 's "aware" of it ,
>> regional to
>> councils as well] three stage filter [pre, HEPA , and carbon to humanize
>> bad
>> breath of wave maintenance guys ; able to discharge, optionally ; air
back
>> to
>> room] ; finally gets overdosed ! And there goes this >six sigma< fellow
in
>> crime "personally" preferring holes {which I'd understood} ; but in roof
>> !!! ;
>> no wonder I get all stuffy trotting seminars round LA !!!
>> You guys work like middle aged England's industrial revolution : Stuff
the
>> pigeons (literally) ; here comes the progress . I understand theyr's
>> etching
>> on your prized 3pack duco and shitting down Acropolis is not quite that
>> nice ;
>> still ; I'm flabbergasted .
>>
>> paul>>
>>
>> Hi ya Paul!
>>
>>      Flabbergasted are ya? Ya' shouldn't be...things aren't quite so bad
>> as
>> the picture you're painting of us...while there's room for improvement to
>> be
>> sure (don't get me started on MTBE's, California's way of dealing with
the
>> pollution of auto exhaust) we're not quite back in the middle ages. A lot
>> of
>> the things I was saying was meant quite "tongue in cheek" and not be
taken
>> literally.
>>
>> Here in the San Fransisco Bay Area we have a quite strict organanization
>> called the Bay Area Air Quality Management District under which all of us
>> printed circuit businesses answer to, and those that have dealt with
>> BAAQMD
>> know what I'm talking about when I say strict....
>>
>> The following is from Regulation 11 (Hazardous Pollutants)
>> Rule 15 (Airborn Toxic Control Measure For Emissions of Toxic Metals From
>> Non-
>> Ferrous Metal Melting)
>>
>> The first part (a) goes through all the definitions, then it gets into
the
>> regulation:
>>
>> (b) Requirements: No person shall operate a non-ferrous metal melting
>> furnace
>> unless the facility is in compliance with all the requirements specified
>> in
>> subsections B1 through B3.
>>
>> The section that really applies to guys like us is:
>>
>> (B3) Fugitive Emission Control
>>
>>         (a) No activity associated with metal melting at a facilty
>> including furnace
>> operation, casting, emission control system operation, and the  storage,
>> handling, transfer of any materials (except new sand) shall discharge
into
>> the
>> air any air contaminate, other than uncombined  water vapor, for a period
>> aggregating more than three minutes in any hour which is:
>>                 (i) Half as dark or darker in shade as that designated as
>> number 1 on the
>> Ringlemann Chart, as published by the United States Bureau
>> of Mines, or
>>                 (ii) Of such opacity as to obscure an observer's view to
a
>> degree equal to
>> or greater than smoke as described in subsection B3, A(i) or
>> 10% opacity.
>>
>>         (b) Dust-forming material including, but not limited to, dross,
>> ash, or feed
>> material shall be stored in an enclosed storage area or stored in a
>> manner
>> which meets the requirements of subsection B3 (a).
>>
>>         (c) Material collected by a particulate matter control system
>> shall be
>> discharged into closed containers or an enclosed system that is
>> completely
>> sealed to prevent any dust from getting out.
>>
>>         (d) Surfaces that are subjected to vehicular or foot traffic
shall
>> be
>> vacuumed, wet mpped, or otherwise maintained in accordance with a
>> District-
>> approved maintenance plan. The plan shall specify, at a minimum: the
areas
>> to
>> be cleaned, the method to be used, the required         frequency of the
>> cleaning
>> activities, and a method of documenting the completion of the required
>> activities. The plan shall be designed and      carried out in a way
which
>> will
>> meet the requirements of B3 (a)
>>
>> (C) Exemptions
>>
>>         1) Small Quantity Exemptions.
>>
>>         Facilities are exempt from subsections B1, B2, and B3 if they
meet
>> either of
>> the following conditions:
>>
>>                 (a) Melt a total of no more than one ton per year of all
>> metals, or
>>                 (b) Melt no more than the listed quantities of any one of
>> the specific
>> metals listed in table 1.
>>
>>
>> TABLE 1
>>
>>         METAL
>> EXEMPTION LIMIT (Tons per year)
>>
>>         Pure Lead
>> 400
>>         Hard Lead
>> 200
>>         Aluminum Scrap
>> 125
>>         Aluminum Ingot containing more
>> 125
>>         than .004% cadmium or .002%
>>         arsenic
>>         Solder
>> 100
>>         Zinc Scrap
>> 30
>>         Copper or Copper based alloys
30
>>         containing more than .004% cadmium
>>         0r .002% arsenic
>>         Type Metal (lead for linotype machines)         25
>>
>> So as you can see, by following the regulations there's a lot of us small
>> guys
>> exempt. Sorry things are so tough for you down under. I'm no
environmental
>> engineer, but do you really think all the regulations that you have to
>> deal
>> with are really necessary?
>>
>> I'm not going to try and debate that lead isn't a toxic compound, and if
>> it
>> were a perfect world there shouldn't be anything harmful to us humans
>> anywhere, but sometimes regulations can be "overkill", just as I'm sure
>> regulations can be ineffective sometimes. I'm just asking the questions
of
>> what is really prudent and neccesary?
>>
>> As far as you always being stuffed up down in LA, I'm pretty sure you can
>> blame that on the weather patterns, the geography of the LA Basin, and
>> cars.
>> Not my reflow and wave exhaust...I wouldn't do that to ya' pardner!
>>
>> -Steve Gregory-
>>
>> ################################################################
>> TechNet E-Mail Forum provided as a free service by IPC using LISTSERV
1.8c
>> ################################################################
>> To subscribe/unsubscribe, send a message to [log in to unmask] with
>> following text in the body:
>> To subscribe:   SUBSCRIBE TechNet <your full name>
>> To unsubscribe:   SIGNOFF TechNet
>> ################################################################
>> Please visit IPC's web site (http://www.ipc.org) "On-Line Services"
>> section for additional information.
>> For technical support contact Hugo Scaramuzza at [log in to unmask] or
>> 847-509-9700 ext.312
>> ################################################################
>>
>
>################################################################
>TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
>################################################################
>To subscribe/unsubscribe, send a message to [log in to unmask] with following
text in the body:
>To subscribe:   SUBSCRIBE TechNet <your full name>
>To unsubscribe:   SIGNOFF TechNet
>################################################################
>Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section
for additional information.
>For technical support contact Hugo Scaramuzza at [log in to unmask] or
847-509-9700 ext.312
>################################################################
>
>

################################################################
TechNet E-Mail Forum provided as a free service by IPC using LISTSERV 1.8c
################################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in the body:
To subscribe:   SUBSCRIBE TechNet <your full name>
To unsubscribe:   SIGNOFF TechNet 
################################################################
Please visit IPC's web site (http://www.ipc.org) "On-Line Services" section for additional information.
For technical support contact Hugo Scaramuzza at [log in to unmask] or 847-509-9700 ext.312
################################################################


ATOM RSS1 RSS2