TECHNET Archives

May 2002

TechNet@IPC.ORG

Options: Use Monospaced Font
Show HTML Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Charles Caswell <[log in to unmask]>
Date:
Thu, 9 May 2002 10:27:11 -0700
Reply-To:
"TechNet E-Mail Forum." <[log in to unmask]>, David Douthit <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset=us-ascii; x-mac-type="54455854"; x-mac-creator="4D4F5353"
From:
David Douthit <[log in to unmask]>
Parts/Attachments:
text/plain (63 lines)
Charles,

The over spray flux may not be exposed to enough heat to "activate" the chemistry.
This residual "raw" flux can be very ionic!

David A. Douthit
Manager
LoCan LLC

Charles Caswell wrote:

> If you are using no-clea, and presumably not cleanig, why would a little flux topside be of concern? I do not use no-clean but am inetrested.
> Charles Caswell
>
> -----Original Message-----
> From: David White [mailto:[log in to unmask]]
> Sent: Thursday, May 09, 2002 9:33 AM
> To: [log in to unmask]
> Subject: [TN] Flux on top of PCBs from wave
>
> Technet,
> Is anyone concerned about the over spray of flux on the top of PCB
> assemblies. We use generic pallets in our process, so our PCB's will get
> over spray form the spray fluxer, it has recently been brought up as a
> concern.  We use a no-clean flux (Lonco SLS65).  Does anyone else do this
> also, and if so do you have the same concerns?  The flux can sometimes be
> pretty noticeable. I am in the process of getting Ionic testing done, but
> would like your experiences.
> Dave
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------
>
> ---------------------------------------------------------------------------------
> Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
> To unsubscribe, send a message to [log in to unmask] with following text in
> the BODY (NOT the subject field): SIGNOFF Technet
> To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
> To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
> Search the archives of previous posts at: http://listserv.ipc.org/archives
> Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
> information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
> ---------------------------------------------------------------------------------

---------------------------------------------------------------------------------
Technet Mail List provided as a free service by IPC using LISTSERV 1.8d
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/html/forum.htm for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-509-9700 ext.5315
---------------------------------------------------------------------------------

ATOM RSS1 RSS2