TECHNET Archives

November 2006

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Date:
Fri, 17 Nov 2006 18:14:49 -0800
Reply-To:
TechNet E-Mail Forum <[log in to unmask]>, [log in to unmask]
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
quoted-printable
Content-Type:
text/plain; charset="us-ascii"
From:
Steven Hoffner <[log in to unmask]>
Parts/Attachments:
text/plain (34 lines)
All,
 
I have a few questions regarding the cleaning of no clean fluxes.  First
I know this is not recommended but I have a number of power supply
assemblies (120/240V in, 3.3V out) that were poorly cleaned.
 

1.      Are the Sn and Pb salts left on the board conductive on their
own in a low humidity (less than 50%) environment?
2.      What level of Cl, Br, SO, NO, Weak Organic Acid contaminants if
detected using Ion Chromatography would be low risk?
3.      What are some tests, that can quantify risk, that can be made on
actual assemblies?
4.      What tests are best to screen any potential infant mortality
failures?
5.      What are the best ways to clean the No clean flux residues from
the assemblies?

TIA,
Steven Hoffner 


 

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2