Scott,
With a wedge bonder, you will have two options -
Place one bond next to the other [leaving room between the bonds for the
bonding tool]. You really can not literally stack the bonds with the
wedge bonder. Unfortunately, you are not likely to have room enough on
your pad to accomplish this.
Or use what is called a multiple stitch bonds [or just 'stitch' bond].
Make your first bond then go to the second bond site and bond without
'wedging off' and continue the bond to the next site without breaking
the wire between the first and third bonds.
Most every heavy wire wedge bonder can do this, but there will be some
layout constraints. Your 'pad' may need to be in-line with the two
other bond sites.
Steve
-----Original Message-----
From: TechNet [mailto:[log in to unmask]] On Behalf Of Gold, Scott
Sent: Wednesday, September 03, 2008 2:43 PM
To: [log in to unmask]
Subject: [TN] Overlapping Wire Bonds
Curious here. Can you lay bonds on top of each other. I want to create
1 bond. Then from that same point, start another bond. I need to
connect 2 places from 1 pad (the pad is only 2x the size of the wire).
In this case its .012" AL wire.
Thanks.
--Scott
Scott Gold
Product Development Manager
ECT - Clifton Park, NY
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text
in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to
[log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to
[log in to unmask]: SET Technet Digest
Search the archives of previous posts at:
http://listserv.ipc.org/archives
Please visit IPC web site
http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional
information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100
ext.2815
-----------------------------------------------------
THE INFORMATION CONTAINED IN THIS E-MAIL MESSAGE AND ANY ATTACHMENTS SENT FROM GENTEX CORPORATION IS GENTEX CONFIDENTIAL INFORMATION INTENDED ONLY FOR THE PERSONAL USE OF THE INDIVIDUAL OR ENTITY NAMED ABOVE. If you are not the intended recipient, you are hereby notified that any review, distribution, or copying of this communication is strictly prohibited. If you have received this communication in error, please immediately notify the sender by return e-mail, and delete this e-mail message and any attachments from your computer. [gntx v.1]
---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 15.0
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------
|
|
|