TECHNET Archives

September 2005

TechNet@IPC.ORG

Options: Use Proportional Font
Show Text Part by Default
Show All Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Subject:
From:
Stephen R Gregory <[log in to unmask]>
Reply To:
TechNet E-Mail Forum <[log in to unmask]>, Stephen R Gregory <[log in to unmask]>
Date:
Tue, 20 Sep 2005 08:24:33 -0500
Content-Type:
text/plain
Parts/Attachments:
text/plain (69 lines)
                                Hi Richard!

                                We have a few boards that call out that too. From my point of
                                view, as far as appearance, it looks the same as HASL.

                                I've tried to think why Fused tin/lead would be called out instead
                                of HASL, and my only guess is that someone didn't want the boards
                                to be themally shocked by the HASL process. I might also add these
                                were on 61-20 layer VME cards where everything was SMT, and the
                                only PTH was press-fit connectors...so the boards didn't even see wave
                                solder.

                                Kind regards,

                                -Steve Gregory-
                                Senior Process Engineer
                                LaBarge Incorporated
                                Tulsa, Oklahoma
                                (918) 459-2285
                                (918) 459-2350 FAX





        "Stadem, Richard" <[log in to unmask]>
                        Sent by: TechNet <[log in to unmask]>
                        09/20/2005 07:51 AM
                        Please respond to TechNet E-Mail Forum <[log in to unmask]>; Please respond to "Stadem, Richard" <[log in to unmask]>
                                	
        To:     [log in to unmask]@SMTP@Exchange
        cc:     (bcc: Stephen R Gregory/LABARGE)
        Subject:        [TN] Fused tin lead plating versus HASL	


                                Hi, folks
                                I have a pwb fab drawing that calls out fused tin-lead plating or solder
                                coating. I know that the solder coating is HASL, but what is fused
                                tin/lead? My understanding is that it is a tin/lead coating that is
                                applied to the bare pwb using a reflow oven process. Does this provide a
                                flat surface of tin/lead? If my only choice of finish is tin/lead, which
                                process is better in terms of flatness and solderability? I have a
                                fine-pitch BGA that is going to be assembled on this pwb.

                                ---------------------------------------------------
                                Technet Mail List provided as a service by IPC using LISTSERV 1.8e
                                To unsubscribe, send a message to [log in to unmask] with following text in
                                the BODY (NOT the subject field): SIGNOFF Technet
                                To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
                                To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
                                Search the archives of previous posts at: http://listserv.ipc.org/archives
                                Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
                                -----------------------------------------------------



                                __________________________________________________________________
                                This message may contain information that is privileged and confidential to LaBarge, Inc.  It is for use only by the individual or entity named above.  If you are not the intended recipient, you may not copy, use or deliver this message to anyone.  In such event, you should destroy the message and kindly notify the sender by reply e-mail.

---------------------------------------------------
Technet Mail List provided as a service by IPC using LISTSERV 1.8e
To unsubscribe, send a message to [log in to unmask] with following text in
the BODY (NOT the subject field): SIGNOFF Technet
To temporarily halt or (re-start) delivery of Technet send e-mail to [log in to unmask]: SET Technet NOMAIL or (MAIL)
To receive ONE mailing per day of all the posts: send e-mail to [log in to unmask]: SET Technet Digest
Search the archives of previous posts at: http://listserv.ipc.org/archives
Please visit IPC web site http://www.ipc.org/contentpage.asp?Pageid=4.3.16 for additional information, or contact Keach Sasamori at [log in to unmask] or 847-615-7100 ext.2815
-----------------------------------------------------

ATOM RSS1 RSS2