The question is why they need to use low melting temp solder - something
else on the board is not allow to be heat up? if so, the finish of the
parts is not a good selection (should get caught during BOM design
review). Just curious.
jk
> Hi Mumtaz - two things we have seen that are important when soldering
> NiPdAu component finishes are (1) soldering temperature/profile. Pd
> dissolves much slower into Sn than other elements so running the soldering
> temperatures 10 degrees hotter than typical and increasing the soldering
> time 3-5 seconds longer than typical can be beneficial; (2) flux
> formulation. Some fluxes work better than others when Pd is included in
> the
> soldering situation. Hope this helps.
>
> Dave Hillman
> Rockwell Collins
> [log in to unmask]
>
> On Thu, Jul 23, 2015 at 10:46 AM, Mumtaz Bora <[log in to unmask]> wrote:
>
>> Dear All, Good Morning, Looking for some knowledge base on soldering
>> NiPdAu finished components with low melt solder such as
>> Sn42.0Bi57.6Ag0.4
>> to avoid wetting issues on a heavy copper plane board. Any insight and
>> advise will be appreciated.
>>
>> Thank-you
>> Mumtaz
>> 858-795-0112
>> Peregrine Semiconductor
>>
>>
>> CONFIDENTIALITY NOTE: The information transmitted, including
>> attachments,
>> is intended only for the person(s) or entity to which it is addressed
>> and
>> may contain confidential and/or privileged material. Any review,
>> retransmission, dissemination or other use of, or taking of any action
>> in
>> reliance upon this information by persons or entities other than the
>> intended recipient is prohibited. If you received this in error, please
>> contact the sender and destroy any copies of this information.
>>
>> ______________________________________________________________________
>> This email has been scanned by the Symantec Email Security.cloud
>> service.
>> For more information please contact helpdesk at x2960 or
>> [log in to unmask]
>> ______________________________________________________________________
>>
>
>
> ______________________________________________________________________
> This email has been scanned by the Symantec Email Security.cloud service.
> For more information please contact helpdesk at x2960 or [log in to unmask]
> ______________________________________________________________________
>
______________________________________________________________________
This email has been scanned by the Symantec Email Security.cloud service.
For more information please contact helpdesk at x2960 or [log in to unmask]
______________________________________________________________________
|
|
|