TECHNET Archives

July 2000

TechNet@IPC.ORG

Options: Use Monospaced Font
Show Text Part by Default
Condense Mail Headers

Message: [<< First] [< Prev] [Next >] [Last >>]
Topic: [<< First] [< Prev] [Next >] [Last >>]
Author: [<< First] [< Prev] [Next >] [Last >>]

Print Reply
Sender:
X-To:
Brooks Bill <[log in to unmask]>
Date:
Tue, 18 Jul 2000 22:16:40 +0100
Reply-To:
Mike Fenner <[log in to unmask]>
Subject:
MIME-Version:
1.0
Content-Transfer-Encoding:
7bit
Content-Type:
text/plain; charset="Windows-1252"
From:
Mike Fenner <[log in to unmask]>
Parts/Attachments:
text/plain (148 lines)
WD 40 and variants are indeed handy solvents, and here comes the but
... the solvents dry off OK leaving oily residue penetrated into all
sorts of places. This will give you a nasty flypaper effect at best.
At worst they are acidic. Probably OK in reducing the odd bit of
corrosion on a stuck nut, but not desirable on a PCB.

Mike


----- Original Message -----
From: "Brooks Bill" <[log in to unmask]>
To: <[log in to unmask]>
Sent: Monday, July 17, 2000 4:35 PM
Subject: Re: [TN] Adhesive Remover for artwork


> There's a little known remover that most of us have in our garage...
WD-40.
> I used it many times to remove masking tape glue residue from glass
on
> tabletops... but remember it's a penetrating oil with petroleum
distillates
> in it... so make sure it won't hurt the object you want to clean...
> - Bill Brooks
>
>
> -----Original Message-----
> From: Dieselberg, Ron [mailto:[log in to unmask]]
> Sent: Monday, July 17, 2000 4:54 AM
> To: [log in to unmask]
> Subject: Re: [TN] Adhesive Remover for artwork
>
>
> Hans, try "Goo Gone". I use it at home and have seen librarians use
it to
> remove labels from books. It works great! Try a small spot first, as
always.
> Ron Dieselberg
> BAE SYSTEMS
> Cincinnati Electronics Corp.
>
> -----Original Message-----
> From: Hinners Hans Civ WRALC/LYPME
[mailto:[log in to unmask]]
> Sent: Thursday, July 13, 2000 16:41
> To: [log in to unmask]
> Subject: [TN] Adhesive Remover for artwork
>
>
> Hey Gang,
>
> I'm looking for an adhesive remover.
>
> We're using a new label printer to image the batch numbers on the
panels.
> Only problem, the labels are leaving adhesive on the artwork when we
pull
> them off.  I already tried Chemtronics adhesive remover and it just
smeared
> the glue around.  So, before I start making a bunch of calls or
trying
> household cleaners I thought I'd ask this illustrious body.
>
> Thanks,
>
> Hans
>
> ~~~~~~~~~~~~~~~~~~~
> Hans M. Hinners
> Materials (Process & Manufacturing) Engineer
> Warner Robins Air Logistics Center
> Avionics Production Division
> Manufacturing Branch
> 380 Second Street, Suite 104
> Building: 640, Mail Stop: LYPME
> Robins AFB, GA 31098-1638
> Voice: (912) 926 - 1970 Fax: (912) 926 - 7164
> mailto:[log in to unmask]
> http://www.robins.af.mil
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV
1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following
> text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV
1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following
> text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
>
> ##############################################################
> TechNet Mail List provided as a free service by IPC using LISTSERV
1.8c
> ##############################################################
> To subscribe/unsubscribe, send a message to [log in to unmask] with
following text in
> the body:
> To subscribe:   SUBSCRIBE TECHNET <your full name>
> To unsubscribe:   SIGNOFF TECHNET
> ##############################################################
> Please visit IPC web site (http://www.ipc.org/html/forum.htm) for
additional
> information.
> If you need assistance - contact Keach Sasamori at [log in to unmask] or
> 847-509-9700 ext.5315
> ##############################################################
>

##############################################################
TechNet Mail List provided as a free service by IPC using LISTSERV 1.8c
##############################################################
To subscribe/unsubscribe, send a message to [log in to unmask] with following text in
the body:
To subscribe:   SUBSCRIBE TECHNET <your full name>
To unsubscribe:   SIGNOFF TECHNET
##############################################################
Please visit IPC web site (http://www.ipc.org/html/forum.htm) for additional
information.
If you need assistance - contact Keach Sasamori at [log in to unmask] or
847-509-9700 ext.5315
##############################################################

ATOM RSS1 RSS2